26/Mar/2020 | 69022000 | Refractory bricks (containing 80% Aluminum oxide), used for the bottom of ladle-ladle liquid steel pouring during steel casting process, resistant to 1800 degrees Celsius, size: 100WX 150LX300H, new 100% Shaped Refractory LADLE BOTTOM BRICK UCS-3I 30/0-Q4 | China | piece/pcs | 1,080.00 | 15,757.20 | 14.59 | View Importer | View Supplier |
26/Mar/2020 | 69022000 | Refractory brick (containing 58% aluminum oxide), resistant to 1760 degrees Celsius, placed in the corner of the intermediate container for liquid steel casting process, 298.8x100x150, new 100% -Shaped Refractory UCS-2I CONNER BLOCK-Q4421291 | China | piece/pcs | 300.00 | 5,055.00 | 16.85 | View Importer | View Supplier |
28/Jan/2019 | 69022000 | Refractory bricks (containing 60.61% aluminum oxide) , used for intermediate bottom of tanks-Tundish during steel casting , resistant to 1760 degrees C, new products 100% / Shaped refractories UCS-2I 230X150X100 | China | Piece/Pcs | 288.00 | 3,268.80 | 11.35 | View Importer | View Supplier |
28/Jan/2019 | 69022000 | Refractory bricks (containing 60.61% aluminum oxide) , used for intermediate tanks (Tundish) in the casting process of steel, subjected to 1760 degrees Celsius, 400x400x160 , 100% new / Shaped Refractories Brick UCS-2I | China | Piece/Pcs | 32.00 | 2,695.68 | 84.24 | View Importer | View Supplier |
28/Jan/2019 | 69022000 | Refractory bricks (containing 59.10% aluminum oxide) , resistant to 1760 degrees Celsius, used in the corner of the intermediate container for liquid steel casting process , 298.8x100x150 , 100% new -Shaped Refractory UCS-2I CONNER BLOCK | China | Piece/Pcs | 500.00 | 9,360.00 | 18.72 | View Importer | View Supplier |
02/Jan/2019 | 69022000 | Refractory bricks (containing 59.1% aluminum oxide) , used for intermediate boxes (Tundish) in the casting process of steel, subjected to 1760 degrees Celsius, 298.8LX 100W X 150H , 100% new / Shaped Refractories Brick UCS- 2I | China | Piece/Pcs | 220.00 | 4,118.40 | 18.72 | View Importer | View Supplier |