27/Mar/2020 | 38249999 | Iron ladle protective slag, powder, main components SiO2: 25-28%, CaO: 15-25%, MgO: 4-6% ... and inorganic salts, for insulation insulation used in the process of pig iron making, 100% new. | China | ton | 300.00 | 124,500.00 | 415.00 | View Importer | View Supplier |
24/Mar/2020 | 38249999 | Iron ladle protective slag, powder, main components SiO2: 25-28%, CaO: 15-25%, MgO: 4-6% ... and inorganic salts, for insulation insulation used in the process of pig iron making, 100% new. | China | ton | 300.00 | 124,500.00 | 415.00 | View Importer | View Supplier |
19/Mar/2020 | 38160090 | Refractory mortar protects the furnace wall (furnace construction materials). New 100%. SiO2: 51.83%, CaO: 19.85%, Al2O3: 5.32%, MgO: 2.27%, C: 15%, Na2O: 8%. | China | ton | 52.00 | 21,736.00 | 418.00 | View Importer | View Supplier |
16/Mar/2020 | 38160090 | Refractory mortar protects the furnace wall (furnace construction materials). New 100%. SiO2: 51.83%, CaO: 19.85%, Al2O3: 5.32%, MgO: 2.27%, C: 15%, Na2O: 8%. | China | ton | 10.00 | 4,150.00 | 415.00 | View Importer | View Supplier |
26/Jan/2019 | 38249999 | Desiccant preparations , in the form of granules , whose main components are: 70% calcium oxide and 15% polyethylene, packed 5kg / bag , 100% new | China | Ton | 26.00 | 10,920.00 | 420.00 | View Importer | View Supplier |
25/Jan/2019 | 38249999 | Chemical preparations used in the metallurgical industry (used to separate oxygen from steel billets) , component Ca: 30-40%; AL: 5-10%; Si: 4-15%; Mg: 1-6%; F: 1-5%; C 8-16%. 100% new | China | Ton | 31.00 | 8,954.12 | 288.84 | View Importer | View Supplier |
09/Jan/2019 | 38231990 | Materials used to paint: Refined Oleic Acid ((A mixture of fatty acids including oleic acid (~ 21 , 8%) , linoleic acid (~ 45%) , palmitic acid (~ 15 , 5%) , stearic acid (~ 5 , 21%) , liquid)) , brand new 100%. | China | Ton | 20.00 | 18,200.00 | 910.00 | View Importer | View Supplier |
04/Jan/2019 | 38249999 | Moisture-proof preparations, in the form of granules , whose main components are: 70% calcium oxide and 15% polyethylene, packed 5kg / bag , 100% new | China | Ton | 20.00 | 8,400.00 | 420.00 | View Importer | View Supplier |
03/Jan/2019 | 38231990 | Materials used to paint: Refined Oleic Acid ((A mixture of fatty acids including oleic acid (~ 21 , 8%) , linoleic acid (~ 45%) , palmitic acid (~ 15 , 5%) , stearic acid (~ 5 , 21%) , liquid)) , brand new 100%. | China | Ton | 20.00 | 18,200.00 | 910.00 | View Importer | View Supplier |
03/Jan/2019 | 38249999 | Cast iron water tank protection agent, in powder form , the main component is silicon oxide , inorganic salts (SiO2: 25-28% , CaO: 15-25% , MgO: 4-6% ... ) to insulate for use in iron casting , 100% new | China | Ton | 100.00 | 41,500.00 | 415.00 | View Importer | View Supplier |