26/Jan/2019 | 69022000 | Refractory bricks containing more than 50% by weight are a mixture of silicon dioxide and aluminum oxide , refractory> = 1770 degrees Celsius, kt: (230-460x114-250x45-65) mm + -3%. New 100% .LIUPAN SHUIJUFENG REFRACTORY MATERIAL CO. , LTD SX | China | Kg | 7,377.00 | 1,844.25 | 0.25 | View Importer | View Supplier |
23/Jan/2019 | 69022000 | Refractory bricks containing more than 50% by weight are a mixture of silicon dioxide and aluminum oxide , refractory> = 1770 degrees Celsius, kt: (230-460x114-250x45-65) mm + -3%. New 100% .LIUPAN SHUIJUFENG REFRACTORY MATERIAL CO. , LTD SX | China | Kg | 28,750.00 | 7,187.50 | 0.25 | View Importer | View Supplier |
16/Jan/2019 | 69022000 | Refractory bricks containing more than 50% by weight are a mixture of silicon dioxide and aluminum oxide , refractory> = 1770 degrees Celsius, kt: (200-280x100-230x25-65) mm + -3%. New 100% .LIUPAN SHUIJUFENG REFRACTORY MATERIAL CO. , LTD SX | China | Kg | 9,700.00 | 2,425.00 | 0.25 | View Importer | View Supplier |