27/Mar/2020 | 38249999 | Iron ladle protective slag, powder, main components SiO2: 25-28%, CaO: 15-25%, MgO: 4-6% ... and inorganic salts, for insulation insulation used in the process of pig iron making, 100% new. | China | ton | 300.00 | 124,500.00 | 415.00 | View Importer | View Supplier |
24/Mar/2020 | 38249999 | Iron ladle protective slag, powder, main components SiO2: 25-28%, CaO: 15-25%, MgO: 4-6% ... and inorganic salts, for insulation insulation used in the process of pig iron making, 100% new. | China | ton | 300.00 | 124,500.00 | 415.00 | View Importer | View Supplier |
16/Mar/2020 | 38249999 | Liquid steel insulation, powder, intermediate container protection, main component SiO2 = 2.65%; Al2O3 = 31.45%; CaO = 52.23%, used to insulate water of intermediate steel tanks and cast steel plates, 100% new goods | China | ton | 40.00 | 21,600.00 | 540.00 | View Importer | View Supplier |
02/Mar/2020 | 38249999 | Steel tank protector, whose main components are (CaO = 30-40%, SiO2 = 25-30%, MgO = 8-12%, Al2O3 = 12-16%, CaF2 = 7.5%) are used to insulation steel water tanks, 100% new goods | China | ton | 100.00 | 41,500.00 | 415.00 | View Importer | View Supplier |
29/Jan/2019 | 38249999 | Steel ladle protactive slag. Insulation slag is used to cover the surface of steel water , keep heat for steel water tanks , used for steel billet factory , component SiO2 25-30% , CaO 30-40% , Al2O3 12-16 %,new 100% | China | Ton | 24.00 | 9,360.00 | 390.00 | View Importer | View Supplier |