26/Mar/2020 | 26011110 | Unburnt iron ore, Kumba standard type, Fe content accounts for 64.95%, particle size <6.3mm accounts for 80.90%, used as raw material for iron and steel production - blast furnace technology | South Africa | ton | 49,704.14 | 4,474,864.08 | 90.03 | View Importer | View Supplier |
25/Mar/2020 | 26151000 | Zircon ore, sand granular form, ZrO2 content> 65%, grain size> 75 micrometres, packed in 25kg / bag, used for making molds: Zircon sand uncalcined prime grade. New 100%. | South Africa | kg | 8,000.00 | 14,000.00 | 1.75 | View Importer | View Supplier |
09/Mar/2020 | 26011190 | Iron Ore Lumpy iron ore, unburnt type, used as a test sample to be a raw material for the process of pig iron and steel works includes: Fe2O3 = 65.71%, grain size> 6.3mm = 90% | South Africa | kg | 200.00 | 200.00 | 1.00 | View Importer | View Supplier |