28/Jan/2019 | 69021000 | Refractory bricks (containing 68.34% Magnesium oxide) , used for ladle-Ladle wall in the casting process of steel, subjected to 1760 degrees C, 230HX230Lx60Wx80W , 100% new / shaped refractory Brick YMA-10WB LW-232 | China | Piece/Pcs | 1,280.00 | 18,816.00 | 14.70 | View Importer | View Supplier |
28/Jan/2019 | 69021000 | Refractory bricks (containing 77.08% magnesium oxide) , used for ladle-ladle wall in the casting process of steel, subjected to 1760 degrees Celsius, size: 150H x 230L x 80W , 100% new / shaped refractories BRICK YGM -15S1 LW150 | China | Piece/Pcs | 576.00 | 7,418.88 | 12.88 | View Importer | View Supplier |
28/Jan/2019 | 69021000 | Refractory bricks (containing 79.12% Magnesium oxide) , used for ladle-Ladle wall in the casting process of steel, subjected to 1760 degrees Celsius, size: 230H x 230L x 70W x 80W , 100% new -Shaped refractories BRICK YGM-15S1 LW231 | China | Piece/Pcs | 10,240.00 | 188,928.00 | 18.45 | View Importer | View Supplier |
28/Jan/2019 | 69021000 | Refractory bricks (containing 76.86% magnesium oxide) , used for ladle-Ladle wall in the casting process of steel, subjected to 1760 degrees Celsius, 100% new / shaped refractory brick YGM-15S1 LW180 | China | Piece/Pcs | 160.00 | 2,468.80 | 15.43 | View Importer | View Supplier |
02/Jan/2019 | 69021000 | Refractory bricks (containing 68.97% Magnesium oxide) , used for ladle-Ladle wall during casting of steel, subjected to 1760 degrees C, 60W X 80W X 230H X 230L , 100% new -Shaped refractories BRICK YMA- 10WA LW232 | China | Piece/Pcs | 128.00 | 2,036.48 | 15.91 | View Importer | View Supplier |